Optical metrology is providing more information, faster, about surfaces that were once impossible to measure and understand.

When an engineer includes a surface finish specification on a print, the intent is usually not just for aesthetics. Surface finish affects how a part will fit, wear, reflect light, transmit heat, distribute lubrication and accept coatings. The finish should be determined by the part's function: A surface should fulfill the engineering requirements of the application without wasting time and effort on a higher quality finish than necessary. In fact, many applications do better with a certain amount of "texture," and too fine of a finish can be just as bad as too coarse of a finish.

In the 1940s, the surface finish measurement upgraded from visually comparing patch reference standards to moving a fine stylus across a part’s surface via a transducer and amplifier. This provided part measurement data that could be recorded and analyzed against various surface parameters to evaluate its roughness, profile and waviness.

For the next half century, this technique was invaluable to various industries: It helped engines last longer, improved fuel economy, made aircraft safer and offered a host of other improvements in manufacturing. The benefits were valuable industry wide but also to the user, who could obtain results with low-cost, simple-to-operate, portable systems that could be used at the point of manufacture by the machine tool operator.

Measurement results were 2D, meaning that surfaces were analyzed for roughness along a single line, and thus, only a small sample of the surface was actually being inspected. Systems that are more complex would create 3D-surface-area results by combining multiple traces, but there was still a lot of important surface information that could be missed with this mechanical measurement. The key limitation of these systems was that the technique was often limited to parts or structures that were visible and regular (homogeneous) in their surface pattern.



However, there are many surface applications in which a tactile probe may not work. This can include very small surfaces; materials that are very delicate and could be damaged when touched with a probe; surfaces that are coated or irregular (inhomogeneous) in their pattern; or surfaces that are porous, such as ceramics or castings.

As a result, metrology is going through a revolution with a completely new industry developed around optics for true surface analysis.

Moving beyond form, waviness and roughness, optical 2D and 3D analysis now allows for grain structure, lattice and molecular structures on surfaces that were either too small or too delicate for other means of analysis. New surface analysis techniques are being provided by optical technologies using vision, confocal image analysis and interferometry.

Small or sensitive surfaces can be measured using optical 2D profile analysis similar to contact systems with excellent correlation to tactile techniques. These systems can be faster than contact systems and enable profiling of small areas of the surface in an X-Y pattern to create patches for structure analysis. These small patches are often connected (stitched) together to create a larger picture of the sample’s surface. Thus, the combination of these small patches and the system’s longer measuring ranges enable large parts such as bone screws, semiconductors, printing rolls or even portions of an engine block to be inspected and analyzed quickly and accurately with a non-contact surface system and better tools for analyzing the results.

Alternatively, fine images of the surface can be taken and combined in the same manner to produce high-resolution pictures of the surface for analysis.

Because the technology has moved to 3D, ISO 25178 and ASME B46.1 created new areal parameters to standardize the results from these measuring techniques. These include:

The rapidly changing technology is providing more information, faster, about surfaces that were once impossible to measure and understand. These new tools improve the manufacturing and inspection process for the automotive, medical, electronics and other industries.

While countersunk and chamfered holes are similar in appearance, functionally they are quite different. Consequently, different gages exist to serve these different functional requirements.

3 Way Joint Closure

A laser scanning system helps this shop capture the free-form surfaces on a hand-sculpted original. The resulting digitized models are the basis for CAM applications such as programming a CNC machining center. 

Optical Microscope, Fiber Optic Microscope, Optical Inspection - Eternal Science,https://www.fibereye2.com/